镍基高温合金
Incoloy 909
Incoloy Alloy 909,属 Incoloy(因科洛伊)系。合金类型:Precipitation Strengthened Alloy。主要合金元素:镍、铁、钴。牌号对照:UNS N19909。公开资料列的适用行业:航空航天。
UNS N19909英科洛伊 Incoloy 系镍基合金高温合金耐蚀合金
化学成分%
成分明细(%)
| 元素 | 含量(%) | 名称 |
|---|---|---|
| S | ≤0.015 | 硫 |
| Si | 0.25~0.50 | 硅 |
| C | ≤0.06 | 碳 |
| Mn | ≤1.00 | 锰 |
| P | ≤0.015 | 磷 |
| B | ≤0.012 | 硼 |
| Co | 12.0~16.0 | 钴 |
| Nb | 4.30~5.20 | 铌 |
| Ta | ≤0.05 | 钽 |
| Al | ≤0.15 | 铝 |
| Ti | 1.30~1.80 | 钛 |
| Cu | ≤0.50 | 铜 |
| Fe | 36.3~46.9 | 铁 |
| Cr | ≤1.0 | 铬 |
| Ni | 35.0~40.0 | 镍 |
条形长度 = 该元素含量百分比;窄段(<0.8%)未在条上显示,见上表。成分区间以执行标准与随货材质证明书为准。
牌号与性能概览

Incoloy Alloy 909,属 Incoloy(因科洛伊)系。合金类型:Precipitation Strengthened Alloy。主要合金元素:镍、铁、钴。牌号对照:UNS N19909。公开资料列的适用行业:航空航天。
物理性能
| 密度 | 8.19 g/cm³ |
|---|---|
| 熔化范围 | 1395 · 1430 °C |
PROPERTIES
力学性能
按形态与测试温度给出的典型值;实际以执行标准与随货材质证明书为准。
| Temperature °F | Temperature °C | Yield Strength (0.2% Offset) ksi | Yield Strength (0.2% Offset) MPa | Tensile Strength ksi | Tensile Strength MPa | Elongation % | Reduction of Area % |
|---|---|---|---|---|---|---|---|
| Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 | Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 | Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 | Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 | Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 | Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 | Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 | Typical Tensile Properties of Age-Hardened INCOLOY alloy 909 |
| 70 | 20 | 150 | 1034 | 185 | 1276 | 15 | 30 |
| 1200 | 650 | 125 | 862 | 150 | 1034 | 25 | 60 |
| Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures | Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures | Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures | Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures | Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures | Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures | Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures | Room-Temperature Tensile Properties of Age-Hardened Material After 1000-h Exposure to Elevated Temperatures |
| No Exposure | No Exposure | 148 | 1020 | 190 | 1310 | 16 | 32 |
| 1100 | 595 | 159 | 1096 | 195 | 1345 | 12 | 29 |
执行标准
| 标准体系 / 形态 | 标准号与说明 |
|---|---|
| UNS | N19909 |
| SAE AMS 5884 | Billets |
| SAE AMS 5892 | Bars & Forgings |
| SAE AMS 5893 | Sheet & Strip |
典型应用
公开资料所列行业:航空航天。具体部件与工况:待补。
工艺与焊接要点
· 强化方式:Precipitation Strengthened Alloy。 · 工艺细节(热处理制度/焊接/加工)与耐蚀定量数据:待补——须以 ASTM/AMS 标准与厂商手册核实后补入,勿据本条推断。
同系列其他牌号英科洛伊 Incoloy 系
说明:本页成分与性能数据依据公开标准与自有资料整理; 执行标准与验收以 GB/ASTM/AMS 标准及随货质保书为准;所列牌号为行业通用牌号对照, 不代表任何第三方厂商授权或代理关系。
要这个牌号的具体规格与价格?
把牌号、规格、数量与技术要求发来,我们核对可供应状态与检验口径后回复。
手机 13301717224 (唐先生)
总机 021-37789863 · 021-57886082 · 021-57886263
地址 上海市松江区泗泾镇泗砖公路 600 号
已复制,可直接粘贴
提交后我们会尽快回复;急件建议直接来电,把使用时间说清楚, 我们优先判断有没有可行路径。