镍基高温合金

Inconel 725

Inconel Alloy 725,属 Inconel(英科乃尔)系。合金类型:Precipitation Strengthened Alloy。主要合金元素:镍、铬、钼、铌。牌号对照:UNS N07725。公开资料列的适用行业:航空航天、海洋工程、焊接材料。

UNS N07725英科耐尔 Inconel 系镍基合金高温合金

化学成分%

Ni
Cr
Fe
Mo
成分明细(%)
元素含量(%)名称
S≤0.010硫
Si≤0.20硅
C≤0.03碳
Mn≤0.35锰
P≤0.015磷
Nb2.75~4.00铌
Al≤0.35铝
Ti1.00~1.70钛
Fe2.3~14.3铁
Mo7.0~9.5钼
Cr19.0~22.5铬
Ni55.0~59.0镍

条形长度 = 该元素含量百分比;窄段(<0.8%)未在条上显示,见上表。成分区间以执行标准与随货材质证明书为准。

牌号与性能概览

Inconel 725 网络收集材料实拍

Inconel Alloy 725,属 Inconel(英科乃尔)系。合金类型:Precipitation Strengthened Alloy。主要合金元素:镍、铬、钼、铌。牌号对照:UNS N07725。公开资料列的适用行业:航空航天、海洋工程、焊接材料。

物理性能

密度8.31 g/cm³
熔化范围1271 · 1343 °C
泊松比0.31
PROPERTIES

力学性能

按形态与测试温度给出的典型值;实际以执行标准与随货材质证明书为准。

ConditionYield Strength (0.2% Offset) ksiYield Strength (0.2% Offset) MPaTensile Strength ksiTensile Strength MPaElongation %Hardness RcCharpy Impact ft-lbfCharpy Impact J
Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.Round, Transverse specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190 mm) diameter.
Annealed62427124855575
Age Hardened133917180124130366892
Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.Round, Longitudinal specimens from hot-finished rounds of 0.5 to 7.5 in (13 to 190 mm) diameter.
Age Hardened1319031801241313697132
TubeTubeTubeTubeTubeTubeTubeTubeTube

执行标准

标准体系 / 形态标准号与说明
UNSN07725
ASTM B983无缝管
ASTM B637Bar and Forgings
ASTM B805棒材/线材
AWS A5.14 ERNiCrMo-15焊丝

典型应用

公开资料所列行业:航空航天、海洋工程、焊接材料。具体部件与工况:待补。

工艺与焊接要点

· 强化方式:Precipitation Strengthened Alloy。 · 工艺细节(热处理制度/焊接/加工)与耐蚀定量数据:待补——须以 ASTM/AMS 标准与厂商手册核实后补入,勿据本条推断。

说明:本页成分与性能数据依据公开标准与自有资料整理; 执行标准与验收以 GB/ASTM/AMS 标准及随货质保书为准;所列牌号为行业通用牌号对照, 不代表任何第三方厂商授权或代理关系。

要这个牌号的具体规格与价格?

把牌号、规格、数量与技术要求发来,我们核对可供应状态与检验口径后回复。

手机 13301717224 (唐先生)

总机 021-37789863 · 021-57886082 · 021-57886263

地址 上海市松江区泗泾镇泗砖公路 600 号

已复制,可直接粘贴

提交后我们会尽快回复;急件建议直接来电,把使用时间说清楚, 我们优先判断有没有可行路径。

我们不会把您的联络信息用于本询价之外的用途。